Brand: EDIBON | Category: Scientific & Laboratory Equipment

EEFCR is used to study creep in metals and polymers at room and elevated temperature. A constant load is applied to a specimen and extension is recorded over time, giving the primary, secondary and tertiary stages of the creep curve.
| Parameter | Value |
|---|---|
| Dimensions | 700 x 350 x 600 mm approx |
| Weight | 25 kg approx |
| Load arm tensile stress range | 0 to 35 N/mm² |
| Dial indicator range | 0 to 10 mm |
| Dial indicator accuracy | 0.01 mm |
Request an itemised quotation covering the proposed configuration, availability, lead time and agreed supply and support scope.
Share what you know. You can start with your name and a phone number or email; final specifications can follow.
Not sure which configuration you need? Help me choose
Contact Vvon Technologies Limited about EDIBON equipment requirements in Bangladesh.
Phone: +8801805987890 | Email: info@vvon.com.bd
Back to Scientific & Laboratory Equipment
EEF is a rotating bending fatigue machine. A specimen is loaded as a cantilever and rotated so its surface sees alternating stress, and cycles to failure are counted to build up an S-N curve. A computer controlled version, EEFC, is also published.
EBVR is a bench hardness tester covering the Brinell, Vickers and Rockwell methods on one machine. Indenters and loads are changed for each scale so students can compare hardness values obtained by different methods on the same material.
EEICI is a pendulum impact tester for Charpy and Izod tests. The pendulum is released from a set height to break a notched specimen and the absorbed energy is read on a scale, so notch shape and temperature effects can be studied. A 300 J version, EEICI/300, is also published.