Solder

Lake Shore supplies solder for mounting sensors, making electrical connections and heat sinking wire in cryogenic assemblies. Indium foil melts at 430 K and has the highest thermal conductivity of the three at 84 W/(m·K), while Ostalloy melts at 343.16 K for low-temperature joints.

Technical Specifications

ParameterValue
Typesindium foil, high-temperature solder, Ostalloy
Melting point430 K (indium foil), solidus 548 K and liquidus 575 K (high-temperature), 343.16 K (Ostalloy)
Thermal conductivity at 293 K84 W/(m·K) indium foil, 35 W/(m·K) high-temperature, 18.6 W/(m·K) Ostalloy
Composition99.99% pure indium; 90% Pb 10% Sn; 50.0% Bi, 26.7% Pb, 13.3% Sn, 10.0% Cd
Density7.3 g/cm3 indium foil, 10.75 g/cm3 high-temperature, 9.67 g/cm3 Ostalloy
Tensile strength2.61 MPa to 3.55 MPa indium foil, 30 MPa high-temperature

View on manufacturer website

Get a Quote

Request an itemised quotation covering the proposed configuration, availability, lead time and agreed supply and support scope.

Useful details to share

Share what you know. You can start with your name and a phone number or email; final specifications can follow.

Request a Quote

Not sure which configuration you need? Help me choose

Contact Vvon Technologies Limited about Lake Shore equipment requirements in Bangladesh.

Phone: +8801805987890 | Email: info@vvon.com.bd

Back to Nanotechnology

View full category